PROTEK 033 BITUMEN PRIMER

Epoxy resin-based, two-component, solvent-free, self-leveling topcoat epoxy material.

PACKAGING         Palette                                                 

17 kg. 27 Pieces                                                     

30 kg. 18 Pieces

  Download pdf document

Download pdf document

• Storage and assembly areas
• Maintenance workshops, garages
• Multi-storey and underground car parks
• Maintenance hangars
• Beverage and food industry floors
• Hobby areas

The product is two-component and it is recommended to mix the amount to be consumed, taking into account the pot life of the mixture. Excessive mixtures will become unusable after the potlife period ends. In order for the mixture to be homogeneous, care must be taken to ensure that the product temperature is +15°C and above. Mix component A in its own packaging for approximately 2-3 minutes with the help of a mixer with an average speed of 300 rpm. Afterwards, the hardener (component B) should be added into it. Mixing should be done until components A and B have a homogeneous structure.

It is produced in metal buckets of 16+4 kg.

APPEARANCE: Colored liquid
COLOR: Ral colors
DENSITY (A+B) 1.45 ±0.05 g/cm³
MIX RATIO (A+B) 4:1 By weight
KATI MADDE (A+B) %100
MIXING CONTAINER LIFE (+10°C) 80 Minutes
MIXING CONTAINER LIFE (+25°C) 30-35 Minutes
ADHESION TO CONCRETE >1.5 N/mm²
HARDNESS (SHORE D) 75 – 80 (after 7 days)
WAITING TIME BETWEEN COATS 8 – 12 Hours
TRANSITION TO LIGHT USE 12 – 24 Hours
7 Days to FULL DRY

Liner:

Make sure a continuous, non-porous layer covers the surface. If necessary, apply two coats of primer. It can be applied with a brush, roller or squeegee. The preferred application is to use a squeegee and go over it with a roller.
Flat wear layer:

Epoxy Self is poured onto the surface and spread with a notched trowel. After spreading the material evenly on the surface, the final coat is obtained by combing it in the X and Y directions with the help of a hedgehog roller.